Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrason® S 2010 G6 UN - PSU-GF30 - BASF

Material Data Center offers the following functions for Ultrason® S 2010 G6 UN:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Ultrason S datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Medium viscosity injection moulding grade with high rigidity and strength, 30 % glass fiber reinforced
Abbreviated designation according to ISO 1043: PSU-GF30
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 30 / * cm³/10min ISO 1133
Température 360 / * °C -
Charge 10 / * kg -
Retrait au moulage, parallèle 0.3 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.5 / * % ISO 294-4, 2577
ASTM Data
Retrait au moulage , parallèle 0.003 mm/mm ASTM D 955
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction - / 8900 MPa ISO 527
Contrainte à la rupture - / 125 MPa ISO 527
Déformation à la rupture - / 2.2 % ISO 527
Module de fluage en traction, 1h * / 8600 MPa ISO 899-1
Résistance au choc Charpy, +23°C - / 45 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C - / 50 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C - / 9 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C - / 9 kJ/m² ISO 179/1eA
ASTM Data
Résistance de traction à la rupture 126 / - MPa ASTM D 638
Allongement à la rupture 1.8 / - % ASTM D 638
Module de flexion 10200 / - MPa ASTM D 790
Izod choc avec entaille, 1/8 in 10 / - J/m ASTM D 256
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de transition vitreuse, 10°C/min 187 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 185 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 187 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 190 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 20 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-1 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Yellow Card disponible oui / * - -
Inflammabilité pr. épaisseur h V-0 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 3.0 / * mm -
Yellow Card disponible oui / * - -
Aptitude à l'allumage 37.4 / * % ISO 4589-1/-2
ASTM Data
DTUL à 66 psi 186 °C ASTM D 648
DTUL à 264 psi 183 °C ASTM D 648
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz * / 3.7 - IEC 62631-2-1
Permittivité relative, 1MHz * / 3.7 - IEC 62631-2-1
Facteur de pertes, 100Hz * / 10 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz * / 60 E-4 IEC 62631-2-1
Résistivité transversale * / >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle * / >1E15 Ohm IEC 62631-3-2
Rigidité diélectrique * / 45 kV/mm IEC 60243-1
Indice de résistance au cheminement * / 125 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 0.6 / * % Sim. to ISO 62
Absorption d'humidité 0.2 / * % Sim. to ISO 62
Masse volumique 1460 / - kg/m³ ISO 1183
Densité 1490 kg/m³ ASTM D 792
Propriétés spécifiques à la matièresec / condUnitéNorme du test
ISO Data
Indice de viscosité 63 / * cm³/g ISO 307, 1157, 1628
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 140 °C -
Pré-séchage - temps 4 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 350 - 390 °C -
Température du moule 130 - 180 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Ultrason® S 2010 G6 UN, PSU-GF30, BASF
Contrainte de cisaillement / Vit. de cisaillement , Ultrason® S 2010 G6 UN, PSU-GF30, BASF
Module de cisaillement dynamique / Température , Ultrason® S 2010 G6 UN (sec), PSU-GF30, BASF
Contrainte / Déformation , Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Module sécant / Déformation , Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Contrainte / Déformation (isochrone) 23°C, Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Module de fluage / Temps 23°C, Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Courbe de fluage 23°C, Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Contrainte / Déformation (isochrone) 140°C, Ultrason® S 2010 G6 UN (sec), PSU-GF30, BASF
Module de fluage / Temps 140°C, Ultrason® S 2010 G6 UN (sec), PSU-GF30, BASF
Courbe de fluage 140°C, Ultrason® S 2010 G6 UN (sec), PSU-GF30, BASF
Volume spécifique (pvT) , Ultrason® S 2010 G6 UN, PSU-GF30, BASF
Module de traction / Température , Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Fatigue strength , Ultrason® S 2010 G6 UN, PSU-GF30, BASF
Caractéristiques
Transformation
Moulage par injection, Extrusion de profilés, Extrusion de plaques
Conditionnement
Granulés, Couleurs naturelles
Propriétés spéciales
Galvanisable
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, max. allowed water content: .02 %
Pre/Post-processing, Pre-drying, Temperature: 140 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 350 - 390 °C
injection molding, Melt temperature, recommended: 360 °C
injection molding, Mold temperature, range: 130 - 180 °C
injection molding, Mold temperature, recommended: 150 °C
injection molding, Dwell time, thermoplastics: 10 min

Pretreatment
Drying temperature: 130 - 150°C
Drying time: minimum 4h
recommended dryer: vaccum or dry air dryer
maximum moisture: 0,02 - 0,05%

Ultrason® can be injection molded by any type of machinery on the market, provided that the plasticizing unit and the mold temperature control system have been configured appropriately. The machinery manufacturer must be consulted if any doubts exist on the ability of various parts to withstand the high temperatures required (e.g. barrel, barrel head, bolted connections, etc.)

Long residence time in combination with high temperatures should be avoided e.g. by pump out material at regular intervals.
During extended interruptions, the barrel temperature should be lowered to about 250-280°C.

It has been found out that heating to the requested processing temperature and shutting down or lowering the temperature is best carried out in two steps.
First, the barrel temperatures are set at the lower processing temperature range for the particular thermoplastic (340 - 350 °C). As soon as these temperatures have reached a steady state, the material in the barrel is pumped out. Second, the barrel temperature can be set to the required processing temperature or the heaters can be shut down.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com